ASTM A53 B A106 B API 5L varrat nélküli csövek nyomás- és hőmérsékletbesorolásai
Oct 11, 2023
ASTM A53 B A106 B API 5L varrat nélküli csövek nyomás- és hőmérsékletbesorolásai
| NPS - Névleges csőméret / OD - Külső átmérő (mm) / SCH - Ütemezés / WT - Falvastagság (mm) | ||||||
| Hálózati házirend-kiszolgáló | OD | SCH | WT | Temp. (C) | ||
| 204 | 260 | |||||
| Megengedett feszültség (MPa) | ||||||
| 137.9 | 130.3 | |||||
| Maximális megengedett feszültség (MPa) | ||||||
| 1/2 | 21.3 | STD | 40 | 2.77 | 34.5 | 32.6 |
| 3/4 | 26.7 | STD | 40 | 2.87 | 28.1 | 26.5 |
| XS | 80 | 3.91 | 39.4 | 37.2 | ||
| 1 | 33.4 | STD | 40 | 3.38 | 26.3 | 24.8 |
| XS | 80 | 4.55 | 36.3 | 34.3 | ||
| 1 1/4 | 42.2 | STD | 40 | 3.56 | 21.6 | 20.4 |
| XS | 80 | 4.85 | 30.2 | 28.5 | ||
| 160 | 6.35 | 40.6 | 38.4 | |||
| 1 1/2 | 48.3 | STD | 40 | 3.68 | 19.4 | 18.4 |
| XS | 80 | 5.08 | 27.4 | 25.9 | ||
| 160 | 7.14 | 39.8 | 37.6 | |||
| 2 | 60.3 | STD | 40 | 3.91 | 16.4 | 15.5 |
| XS | 80 | 5.54 | 23.7 | 22.4 | ||
| 160 | 8.74 | 38.9 | 36.8 | |||
| 2 1/2 | 73 | STD | 40 | 5.16 | 17.9 | 17 |
| XS | 80 | 7.01 | 24.8 | 23.5 | ||
| 160 | 9.53 | 34.7 | 32.8 | |||
| 3 | 88.9 | STD | 40 | 5.49 | 15.6 | 14.7 |
| XS | 80 | 7.62 | 22 | 20.8 | ||
| 160 | 11.13 | 33.1 | 31.3 | |||
| 4 | 114.3 | STD | 40 | 6.02 | 13.2 | 12.5 |
| XS | 80 | 8.56 | 19.1 | 18 | ||
| 120 | 11.13 | 25.2 | 23.8 | |||
| 160 | 13.49 | 31 | 29.3 | |||
| XXS | 17.12 | 40.4 | 38.2 | |||
| 5 | 141.3 | STD | 40 | 6.55 | 11.6 | 10.9 |
| XS | 80 | 9.53 | 17.1 | 16.1 | ||
| 120 | 12.7 | 23.1 | 21.9 | |||
| 160 | 15.88 | 29.4 | 27.8 | |||
| XXS | 19.05 | 35.9 | 33.9 | |||
| 6 | 168.3 | STD | 40 | 7.11 | 10.5 | 9.9 |
| XS | 80 | 10.97 | 16.5 | 15.6 | ||
| 120 | 14.27 | 21.8 | 20.6 | |||
| XXS | 160 | 18.26 | 28.3 | 26.8 | ||
| 8 | 219.1 | 20 | 6.35 | 7.1 | 6.7 | |
| 30 | 7.04 | 7.9 | 7.5 | |||
| STD | 40 | 8.18 | 9.3 | 8.7 | ||
| 60 | 10.31 | 11.7 | 11.1 | |||
| XS | 80 | 12.7 | 14.6 | 13.8 | ||
| 100 | 15.09 | 17.5 | 16.5 | |||
| 120 | 18.26 | 21.4 | 20.2 | |||
| 140 | 20.62 | 24.3 | 23 | |||
| XXS | 22.23 | 26.4 | 24.9 | |||
| 160 | 23.01 | 27.4 | 25.8 | |||
| 10 | 273.1 | 20 | 6.35 | 5.7 | 5.4 | |
| 30 | 7.8 | 7 | 6.6 | |||
| STD | 40 | 9.27 | 8.4 | 7.9 | ||
| XS | 60 | 12.7 | 11.6 | 11 | ||
| 80 | 15.09 | 13.9 | 13.1 | |||
| 100 | 18.26 | 16.9 | 16 | |||
| 120 | 21.44 | 20 | 18.9 | |||
| XXS | 140 | 25.4 | 24 | 22.7 | ||
| 160 | 28.58 | 27.3 | 25.8 | |||
| 12 | 323.9 | 20 | 6.35 | 4.8 | 4.5 | |
| 30 | 8.38 | 6.4 | 6 | |||
| STD | 9.53 | 7.2 | 6.9 | |||
| 40 | 10.31 | 7.9 | 7.4 | |||
| XS | 12.7 | 9.7 | 9.2 | |||
| 60 | 14.27 | 11 | 10.4 | |||
| 80 | 17.48 | 13.5 | 12.8 | |||
| 100 | 21.44 | 16.8 | 15.8 | |||
| XXS | 120 | 25.4 | 20 | 18.9 | ||
| 140 | 28.58 | 22.7 | 21.4 | |||
| 160 | 33.32 | 26.8 | 25.3 | |||
| 14 | 355.6 | 10 | 6.35 | 4.4 | 4.1 | |
| 20 | 7.92 | 5.5 | 5.2 | |||
| STD | 30 | 9.53 | 6.6 | 6.2 | ||
| 40 | 11.13 | 7.7 | 7.3 | |||
| XS | 12.7 | 8.8 | 8.4 | |||
| 60 | 15.09 | 10.6 | 10 | |||
| 80 | 19.05 | 13.4 | 12.7 | |||
| 100 | 23.83 | 17 | 16 | |||
| 120 | 27.79 | 20 | 18.9 | |||
| 140 | 31.75 | 23 | 21.7 | |||
| 160 | 35.71 | 26.1 | 24.6 | |||
| 16 | 406.4 | 10 | 6.35 | 3.8 | 3.6 | |
| 20 | 7.92 | 4.8 | 4.5 | |||
| STD | 30 | 9.53 | 5.8 | 5.4 | ||
| XS | 40 | 12.7 | 7.7 | 7.3 | ||
| 60 | 16.66 | 10.2 | 9.6 | |||
| 80 | 21.44 | 13.2 | 12.5 | |||
| 100 | 26.19 | 16.3 | 15.4 | |||
| 120 | 30.96 | 19.4 | 18.4 | |||
| 140 | 36.53 | 23.1 | 21.9 | |||
| 160 | 40.49 | 25.8 | 24.4 | |||
| 18 | 457 | 10 | 6.35 | 3.4 | 3.2 | |
| 20 | 7.92 | 4.2 | 4 | |||
| STD | 9.53 | 5.1 | 4.8 | |||
| XS | 30 | 11.13 | 6 | 5.7 | ||
| 12.7 | 6.8 | 6.5 | ||||
| 40 | 14.27 | 7.7 | 7.3 | |||
| 60 | 19.05 | 10.4 | 9.8 | |||
| 80 | 23.83 | 13.1 | 12.3 | |||
| 100 | 29.36 | 16.2 | 15.3 | |||
| 120 | 34.93 | 19.5 | 18.4 | |||
| 140 | 39.67 | 22.3 | 21.1 | |||
| 160 | 45.24 | 25.7 | 24.3 | |||
| 20 | 508 | 10 | 6.35 | 3 | 2.9 | |
| STD | 20 | 9.53 | 4.6 | 4.3 | ||
| XS | 30 | 12.7 | 6.1 | 5.8 | ||
| 40 | 15.09 | 7.3 | 6.9 | |||
| 60 | 20.62 | 10.1 | 9.5 | |||
| 80 | 26.19 | 12.9 | 12.2 | |||
| 100 | 32.54 | 16.2 | 15.3 | |||
| 120 | 38.1 | 19.1 | 18.1 | |||
| 140 | 44.45 | 22.5 | 21.3 | |||
| 160 | 50.01 | 25.5 | 24.1 | |||
| 24 | 610 | 10 | 6.35 | 2.5 | 2.4 | |
| STD | 20 | 9.53 | 3.8 | 3.6 | ||
| XS | 12.7 | 5.1 | 4.8 | |||
| 30 | 14.27 | 5.7 | 5.4 | |||
| 40 | 17.48 | 7.1 | 6.7 | |||
| 60 | 24.61 | 10 | 9.5 | |||
| 80 | 30.96 | 12.7 | 12 | |||
| 100 | 38.89 | 16.1 | 15.2 | |||
| 120 | 46.02 | 19.2 | 18.2 | |||
| 140 | 52.37 | 22 | 20.8 | |||
| 160 | 59.54 | 25.3 | 23.9 | |||